How to practice concept:casting

Attempt a question, record the concept and assumptions, then check the available answer. Rework mistakes after revising the relevant concepts. Topic tags can overlap; review the question context.

Questions 1–10 of 13. Imported answers require independent review unless marked reviewed.

Topic practice 13 questionsPage 1 of 2

Question 30

Open question
MEMCQ1 markNeeds review
In relation to metal casting defects, match the following
Defect
Description
P — Dross
I — Shallow blow found on a flat casting surface
Q — Scab
II — Lighter impurities appear on the top surface of a casting
R — Scar
III — A rough, thin layer of metal, protruding above the casting surface, on top of a thin layer of sand
Your answerChoose one option.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 38

Open question
MEMCQ2 marksNeeds review
Match the mold elements in the casting process with the most suitable function.
Mold element
Function
P. Blind riser
I. Cast with internal cavity
Q. Chill
II. Molten metal reservoir
R. Skim bob
III. Nucleating agent
S. Core
IV. Assisting in faster heat removal from melt
T. Insulating sleeve
V. Removal of impurities
U. Inoculant
VI. Increasing the solidification time
Your answerChoose one option.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 25

Open question
MEMSQ1 markNeeds review
In a metal casting process to manufacture parts, both patterns and moulds provide shape by dictating where the material should or should not go. Which of the option(s) given correctly describe(s) the mould and the pattern?
Your answerSelect all correct options. You can choose more than one.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 19

Open question
MEMCQ1 markNeeds review
Fluidity of a molten alloy during sand casting depends on its solidification range. The phase diagram of a hypothetical binary alloy of components A and B is shown in the figure with its eutectic composition and temperature. All the lines in this phase diagram, including the solids and liquids lines, are straight lines. If this binary alloy with 15 weight % of B is poured into a mould at a pouring temperature of 800 °C, then the solidification range is
Diagram for Mechanical Engineering question 19

Your answerChoose one option.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 27

Open question
MEMSQ1 markNeeds review
Consider sand cast of a cube of edge length

. A cylindrical riser is placed at the top of the casting. Assume solidification time,

, where

is the volume and

is the total surface area dissipating heat. If the top of the riser is insulated, which of the following radius/radii of riser is/are acceptable?
Your answerSelect all correct options. You can choose more than one.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 36

Open question
MENAT2 marksNeeds review
A true centrifugal casting operation needs to be performed horizontally to make copper tube sections with outer diameter of 250 mm and inner diameter of 230 mm. The value of acceleration due to gravity,

m/s

. If a G-factor (ratio of centrifugal force to weight) of 60 is used for casting the tube, the rotational speed required is ______ rpm (round off to the nearest integer).

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 37

Open question
MENAT2 marksNeeds review
A cast product of a particular material has dimensions 75 mm × 125 mm × 20 mm. The total solidification time for the cast product is found to be 2.0 minutes as calculated using Chvorinov’s rule having the index,

= 2. If under the identical casting conditions, the cast product shape is changed to a cylinder having diameter = 50 mm and height = 50 mm, the total solidification time will be ____________ minutes (round off to two decimal places).

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 13

Open question
MEMCQ1 markNeeds review
In a casting process, a vertical channel through which molten metal flows downward from pouring basin to runner for reaching the mold cavity is called
Your answerChoose one option.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 50

Open question
MENAT2 marksNeeds review
The figure shows a pouring arrangement for casting of a metal block.
Diagram for Mechanical Engineering question 50

Frictional losses are negligible. The acceleration due to gravity is 9.81 m/s². The time (in s, round off to two decimal places) to fill up the mold cavity (of size 40 cm × 30 cm × 15 cm) is _____

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 13

Open question
MEMCQ1 markNeeds review
During solidification of a pure molten metal, the grains in the casting near the mould wall are
Your answerChoose one option.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer