How to practice Mineral Processing and Extractive Metallurgy

Attempt a question, record the concept and assumptions, then check the available answer. Rework mistakes after revising the relevant concepts. Topic tags can overlap; review the question context.

Questions 1–6 of 6. Imported answers require independent review unless marked reviewed.

Topic practice 6 questionsPage 1 of 1

Question 25

Open question
MTMCQ1 markNeeds review
Which one of the following options is correct?
Red mud is generated in the production of:
Your answerChoose one option.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 41

Open question
MTMCQ2 marksNeeds review
Match the unit operation in Column I with the resulting product in Column II:
Column I (P) COREX Process (Q) Bayer Process (R) Matte Smelting (S) MIDREX Process
Column II (1) Direct Reduced Iron (2) Pig Iron (3) Alumina (4) Copper
Your answerChoose one option.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 47

Open question
MTNAT2 marksNeeds review
Iron powder is compacted at room temperature to 75% of its theoretical density. The as-pressed iron compact is sintered in inert-gas atmosphere at 1200 °C to 90% of its theoretical density. Assuming isotropic shrinkage, the linear shrinkage (in percent) undergone by the iron compact during sintering (rounded off to one decimal place) is ________________ %

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 48

Open question
MTNAT2 marksNeeds review
An alloy having composition W-20 wt % Ni is prepared by mixing elemental powders. The resulting powder mixture is liquid phase sintered at 1550 °C for 1 hour. The liquid phase sintered microstructure consists of interconnected, spherical tungsten grains dispersed in nickel. The tungsten grain size is 70 μm and the W-Ni interparticle neck diameter is 35 μm. If W-Ni interface energy is 0.30 J/m², the W-W interfacial energy (in J/m²), rounded off to two decimal places is ________________
(Given: melting point of W: 3410 °C and melting point of Ni: 1455 °C)

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 62

Open question
MTNAT2 marksNeeds review
A copper ore contains 30 wt.% chalcopyrite (CuFeS₂) and remaining gangue material. Assuming no copper in gangue material, the amount of copper in the ore (rounded off to one decimal place) is __________ wt.%. Given: Atomic weights of Fe, Cu and S are 56, 63.5, and 32 g/mol, respectively.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

Question 64

Open question
MTNAT2 marksNeeds review
Al₂O₃ can be electrolyzed with an inert anode or a carbon anode.
Overall reactions are as follows:
Reaction I: For inert anode,

Reaction II: For carbon anode,

T denotes temperature in Kelvin
Given: Faraday constant = 96500 Coulomb
If inert anode is replaced by carbon anode during electrolysis of Al₂O₃ at temperature 1300 K, the decrease in the magnitude of decomposition potential between the two reactions (rounded off to two decimal places) is __________ Volts.

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer