For a component fabricated from an alloy A with plane strain fracture toughness,
MPa m
, fracture was observed to take place at a crack length of 0.4 mm at a tensile service stress of σ.If the same component is instead fabricated from alloy B with
MPa m
, the crack length at which a similar crack geometry will result in fracture (under identical tensile service stress of σ) is _____ mm (rounded off to one decimal place).Log in to check the answer
You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answerEXPLORE & PRACTISE
Paper and topic context
See where this question comes from and choose what to practise next.
2025MT
GATE MT 2025 · Paper 1
Metallurgical Engineering · Original paper archive
- Section
- Metallurgical Engineering
- Question type
- Numerical answer (NAT)
- Marks
- 2 marks
Practise related topics
Explore more previous year questions using this question’s imported topic tags.
metallurgy
GATE MT previous year questions
materials science
GATE MT previous year questions
materials engineering
GATE MT previous year questions
fracture toughness
GATE MT previous year questions
Fracture behavior, Griffith theory, linear elastic fracture mechanics, fracture toughness, fractography, ductile to brittle transition.
GATE MT previous year questions
Comments
Ask a question, share your approach, or help someone understand.
Log in to view the discussion
You’re not logged in. Log in or create an account to see discussions and add comments.