Question 42: Metal Casting
Give it a try, then reveal the answer to check your work.
Question 42
MTMCQ2 marksNeeds review
Match the casting defects in Column I with the characteristic features in Column II.
Column I
P. Misrun
Q. Expansion scab
R. Pin holes
S. Hot tearing
Column II
Penetration of liquid metal behind surface layer of sand moulds
Metal solidifies prematurely in the mould and some sections of the casting are not filled
Cracking because of restraint to contraction in certain areas of the casting during solidification and cooling to room temperature
Evolution of gases during solidification resulting in porosity
Your answerChoose one option.
Log in to check the answer
You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answerEXPLORE & PRACTISE
Paper and topic context
See where this question comes from and choose what to practise next.
2025MT
GATE MT 2025 · Paper 1
Metallurgical Engineering · Original paper archive
- Section
- Metallurgical Engineering
- Question type
- Multiple choice (MCQ)
- Marks
- 2 marks
Practise related topics
Explore more previous year questions using this question’s imported topic tags.
metallurgy
GATE MT previous year questions
materials science
GATE MT previous year questions
materials engineering
GATE MT previous year questions
casting defects
GATE MT previous year questions
metal casting
GATE MT previous year questions
Comments
Ask a question, share your approach, or help someone understand.
Log in to view the discussion
You’re not logged in. Log in or create an account to see discussions and add comments.