Question 57

MENAT2 marksNeeds review
Two mild steel plates of similar thickness, in butt-joint configuration, are welded by gas tungsten arc weld process using the following weld parameters.
Parameter
Value
Welding voltage
20 V
Welding current
150 A
Welding speed
5 mm/s
A filler wire of the same mild steel material having 3 mm diameter is used in this welding process. The filler wire feed rate is selected such that the final weld bead is composed of 60% volume of filler and 40% volume of plate material. The heat required to melt the mild steel material is 10 J/mm

. The heat transfer factor is 0.7 and melting factor is 0.6. The feed rate of the filler wire is ________ mm/s (round off to one decimal place).

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

EXPLORE & PRACTISE

Paper and topic context

See where this question comes from and choose what to practise next.

2022ME

GATE ME 2022 · Paper 1

Mechanical Engineering · Original paper archive

Section
Mechanical Engineering
Question type
Numerical answer (NAT)
Marks
2 marks

Practise related topics

Explore more previous year questions using this question’s imported topic tags.

mechanical engineering

GATE ME previous year questions

mechanics

GATE ME previous year questions

manufacturing

GATE ME previous year questions

Casting, Forming and Joining Processes

GATE ME previous year questions

welding

GATE ME previous year questions

Comments

Ask a question, share your approach, or help someone understand.

Log in to view the discussion

You’re not logged in. Log in or create an account to see discussions and add comments.