When a metal (M) is immersed in de-aerated acid electrolyte, it polarizes anodically by 0.4 V. The M/M

exchange current density is 10

A m

and Tafel slope is 0.1 V/decade for the anodic reaction. Assume that corrosion is uniform and, anodic and cathodic reactions are under activation control. The rate of metal dissolution in A m

is ________ (round off to 1 decimal place)

Log in to check the answer

You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answer

EXPLORE & PRACTISE

Paper and topic context

See where this question comes from and choose what to practise next.

2021XE-C

GATE XE 2021 · Paper 1

Engineering Sciences · Original paper archive

Section
Section XE-C
Question type
Numerical answer (NAT)
Marks
2 marks

Practise related topics

Explore more previous year questions using this question’s imported topic tags.

engineering sciences

GATE XE previous year questions

engineering

GATE XE previous year questions

applied science

GATE XE previous year questions

degradation materials

GATE XE previous year questions

Degradation of Materials

GATE XE previous year questions

Comments

Ask a question, share your approach, or help someone understand.

Log in to view the discussion

You’re not logged in. Log in or create an account to see discussions and add comments.