GATE MT · 2022 · MT
Question 52: Fatigue
Give it a try, then reveal the answer to check your work.
Question 52
MTNAT2 marksNeeds review
High cycle fatigue data for an alloy at various alternating stresses,
(see figure) is given below.Stress, (MPa) | , Number of cycles to failure |
|---|---|
500 | 1000 |
400 | 10000 |
300 | 100000 |
200 | 1000000 |
![]() |
A specimen of this alloy is subjected to multiple stress cycles sequentially in the following order: (i) first 5000 cycles at
MPa followed by (ii) 25000 cycles at
MPa and finally (iii) at
MPa. Assuming that Miner’s law is obeyed, the number of cycles to failure at the final applied stress of 500 MPa is __________.Log in to check the answer
You can attempt this question now. Sign in to view the answer key, explanations and discussion.Log in to check answerEXPLORE & PRACTISE
Paper and topic context
See where this question comes from and choose what to practise next.
2022MT
GATE MT 2022 · Paper 1
Metallurgical Engineering · Original paper archive
- Section
- Metallurgical Engineering
- Question type
- Numerical answer (NAT)
- Marks
- 2 marks
Practise related topics
Explore more previous year questions using this question’s imported topic tags.
metallurgy
GATE MT previous year questions
materials science
GATE MT previous year questions
materials engineering
GATE MT previous year questions
fatigue
GATE MT previous year questions
high cycle fatigue
GATE MT previous year questions
Comments
Ask a question, share your approach, or help someone understand.
Log in to view the discussion
You’re not logged in. Log in or create an account to see discussions and add comments.